sm_banner

products

OEM Factory for Noble Marble Polishing Powder - FCNS03 Fe Cu Ni Sn Pre Alloyed Powder for Ceramic Diamond Blade – SinoDiam

short description:

FCNS03 Fe Cu Ni Sn Pre Alloyed Powder for Ceramic Diamond Blade 1. What is Pre-alloyed Powder Pre-alloyed powders are harder, less compressible and hence require higher pressing loads to produce high density compacts. However, they are capable of producing high strength sintered materials. Pre-alloying is also used when the production of a homogeneous material from elemental powders requires very high temperatures and long sintering times. The best examples are the stainless steels, whose chr...


Product Detail

Product Tags

Related Video

Feedback (2)

We can constantly satisfy our respected customers with our good high quality, good price tag and good support due to we have been additional specialist and extra hard-working and do it in cost-effective way for Pcd Saw Blade , Lab Grown Diamond Jewelry , Synthetic Diamonds Online , Our final goal is "To try the best, To be the Best". Please feel free to contact with us if you have any requirements.
OEM Factory for Noble Marble Polishing Powder - FCNS03 Fe Cu Ni Sn Pre Alloyed Powder for Ceramic Diamond Blade – SinoDiam Detail:

FCNS03 Fe Cu Ni Sn Pre Alloyed Powder for Ceramic Diamond Blade

1. What is Pre-alloyed Powder

Pre-alloyed powders are harder, less compressible and hence require higher pressing loads to produce high density compacts. However, they are capable of producing high strength sintered materials. Pre-alloying is also used when the production of a homogeneous material from elemental powders requires very high temperatures and long sintering times. The best examples are the stainless steels, whose chromium and nickel contents have to be pre-alloyed to allow economic production by powder metallurgy.

2. The Parameters of FCNS03 

Main Element Fe, Cu, Ni, Sn
Theoretical Density 7.98g/cm³
Sintering Temperature 830℃
Bending Strength 1150Mpa
Hardness 104-108HRB

3. FCNS03 Character

  • The Sintered structure is uniform and compact. the carcass has good control of diamond, great wear resistance and sharpness. 
  • The powder is applied to medium to high quality granite diamond blade, ceramic cutting blades.

4. Instructions for Making Ceramic Cutting Blade.

  1. Metal Percentage:
  • (30-50)% FCNS03 
  • + (25-35)% Cu 
  • + (5-8)% Sn 
  • + (2-4)% Ni
  • + Fe for Blance

   B. Diamond Grit Size and Percentage:

  • 50/60 @ 30%
  • 60/70 @ 40%
  • 70/80 @ 30%
  • Concentration: (9-12)%

    C. Sintering Temperature: 840-860℃


Product detail pictures:

OEM Factory for Noble Marble Polishing Powder - FCNS03 Fe Cu Ni Sn Pre Alloyed Powder for Ceramic Diamond Blade – SinoDiam detail pictures


Related Product Guide:
Wu Jianzhong: Pay attention to innovation, focus on high-end, and promote the transformation and upgrading of superhard industry

Our merchandise are broadly identified and trusted by end users and can satisfy continually developing economic and social requires for OEM Factory for Noble Marble Polishing Powder - FCNS03 Fe Cu Ni Sn Pre Alloyed Powder for Ceramic Diamond Blade – SinoDiam , The product will supply to all over the world, such as: Congo, Israel, Washington, There are advanced producing & processing equipment and skilled workers to ensure the products with high quality. We have found an excellent before-sale, sale, after-sale service to ensure the customers that could rest assured to make orders. Until now our products are now moving on fast and very popular in South America, East Asia, the Middle east, Africa, etc.
  • Reasonable price, good attitude of consultation, finally we achieve a win-win situation,a happy cooperation!
    5 Stars By Samantha from Thailand - 2017.08.28 16:02
    After the signing of the contract, we received satisfactory goods in a short term, this is a commendable manufacturer.
    5 Stars By Sarah from Tunisia - 2017.06.25 12:48
    Write your message here and send it to us